CoorsTek

Home

Contact

Silicon Nitride

Family Overview

Silicon Nitrides (Si3N4) have a unique grain structure which delivers both exceedingly high strength and toughness and exceptionally high thermal shock resistance — making it ideal for applications with high dynamic stresses, thermal rigor, and demanding reliability requirements. Silicon nitrides also have the capacity for high-tolerance, wear-resistant finishes. This unique combination of material properties provides advantages in severe-service applications such as turbines and high-end ball bearings.

  • High toughness
  • Thermal shock resistant
  • Tight tolerances

Hot Pressed Silicon Nitride

By hot pressing silicon nitride, one can achieve nearly zero-porosity. This leads to the exceptional mechanical properties as well as corrosion resistance even in high-temperature applications.

Sintered Silicon Nitride

Sintered silicon nitride's unique grain structure provides excellent mechanical properties for durability in mechanically rigorous environments.

Ceramic Expertise

CoorsTek has broad capabilities for manufacturing Silicon Nitride including specialized manufacturing processes that produce extreme tolerances for optimal performance.

Brochure Downloads

Download the Silicon Nitride Cerbec® Ceramic Balls Brochure

Chemical properties iconElectrical properties iconMechanical properties iconThermal properties icon

Sample Applications by Industry:

Automotive


Semiconductor 

Aerospace & Defense


Energy

Properties Units NBD-200 SN-101C SN-102 SN-103
Flexural Strength, MOR (20 °C) MPa 900 1000 1000 1000
Fracture Toughness, KIc MPa m1/2 5.5 6.5 6.0 6.0

Thermal Conductivity (20 °C)

W/m K 29 34 18 14
Coefficient of Thermal Expansion 1x10-6/°C 2.9 3.7 3.5 3.6
Maximum Use Temperature °C 1400 1400 1000 1000
Dielectric Strength (6.35mm) ac-kV/mm — — 8.6 12
Dielectric Loss (tan δ) 1MHz, 25 °C — — 0.0017 < 0.0004
Volume Resistivity (25°C) Ω-cm

> 1014

> 1014

> 1014

> 1014